- Description
- Quality
- Tips & tricks
- Downloads
Ultrafuse® PP GF30 contains 30% of special glass fibers that are designed for filament making and 3D printing so Ultrafuse® PP GF30 is compatible with any standard FFF printer. PP has a lower moisture uptake than PA. In combination with its high level of glass fiber reinforcement and its excellent chemical resistance, Ultrafuse® PP GF30 is a preferred filament for exceptional working environments. Thanks to its UV resistance it is more suitable than any other PP-based filament for applications directly exposed to sunlight.
Benefits at a glance
- Excellent chemical resistance
- Low density
- Low moisture uptake
- High heat resistance
- Improved UV resistance
We select the best raw materials available from renowned suppliers.
Dedicated people, highest standards.
Production on our state-of-the-art computer controlled machinery guarantees a truly consistent filament, also between colors and batches.
It will perform as expected, every time.
All our products are 100% traceable to the source.
Nozzle Temperature; 240-260 °C
Build Chamber Temperature;-
Bed Temperature; 20-40 °C
Bed modification; PP tape or PPGF adhesive
Drying Procedure;ƒ Dry the filament at 60°C for at least 5 hours
Support Materials;
Nozzle Diamater; 0.6 mm
Print Speed; 30-80 mm/sec